| Product name | Aramid wear-resistant cloth(MKC-KFL041) | ||||
| Composition | |||||
| Raw material | Polyester | 63.3% | |||
| Nylon | 25.6% | ||||
| PU | 11% | ||||
| Specification | Structure | Packaging | |||
| Woven | Roll | ||||
| Properties | Item | Units | Standards | Tolerance | Test method |
| Weight | g/㎡ | 495 | ±25 | ASTM D 3776 | |
| Width | in | 58 | ↑ | ASTM D 3774 | |
| Thickness | mm | 1 | ±0.1 | ASTM D 1777 | |
| Tensile strength | kg/in | L:111 W:43 | min. | ASTM D 5035 | |
| Tearing strength | kg | L:21 W:7 | min. | ASTM D 2261 | |
| Elongation Rate | % | L:40 W:29 | min. | ASTM D 5035 | |
| Abrasion Resistance | cycles | 1500 | Class | ASTM D 3886 | |
| Color Fastness | class | 3 ↑ | min. | AATCC M61 1A | |